Abstract
The purpose of the current study is to evaluate the ageing of poly(ethylene-co-propylene) fittings produced by several manufacturers. The fittings were aged for varying times as follows: 0, 2, 13, 23, 45, 106, 225 and 391 days at 100 ° C. In a previous paper, the oxidation induction time (OItime) and oxidation induction temperature (OItemp) were evaluated with respect to every single step of the ageing process [1] . Here, the Vickers microhardness and wide-angle X-ray line width were used for characterization of the oxidative stability of poly(ethylene-co-propylene) pipes. Both the Vickers microhardness and wide-angle X-ray line width as evaluated from a certain reflex of the diffractogram generally increase with ageing for most samples. The higher microhardness is most likely related to higher fragility of the pipes. The increase of the X-ray line width with ageing indirectly proves that reducing the crystallite size as well as increase of the crystallite defectiveness take place.
- Apostolov, A.A. (2018) On the Oxidation Induction Time and Oxidation Induction Temperature for Characterization of the Oxidative Stability of Poly(Ethylene-Co-Propylene) Pipes. Proceeding of the Bulgarian Academy of Sciences, 71, 38-45.
- Krumova, M., Flores, A., Balta-Calleja, F.J. and Fakirov S. (2002) Elastic Properties of Oriented Polymers, Blends and Reinforced Composites Using the Microindentation Technique. Colloid and Polymer Science, 280, 591-598. https://doi.org/10.1007/s00396-001-0646-z
- Focke, F.W. and van der Westhuizen, I. (2010) Oxidation Induction Time and Oxidation Induction Temperature of Polyethylene in Air. Journal of Thermal Analysis and Calorimetry, 99, 285-293. https://doi.org/10.1007/s10973-009-0097-1
- Krebs, C., Avondet, M-A. and Leu, K.W. (1998) Long Term Behaviour of Thermoplastics—Ageing Behaviour and Chemical Resistance. Hanser-Verlag, Munich.
- Balta Calleja, F. and Fakirov, S. (2000) Microhardness of Polymers. Cambridge University Press, Cambridge. www.cambridge.org/9780521642187
- Wening, W. and Schoeller, T. (1991) Zusammenhange zwischen mechanischem Verhalten und Morphologie von eigenfaserverstarkten Poly(propylen)/Poly(l-buten)-Blends, kristallisiert aus der hochorientierten Schmelze. Angewandte Makromolekulare Chemie, 192, 183-197. https://doi.org/10.1002/apmc.1991.051920115
- Martinez-Salazar, J., Garcia Tijego, J.M. and Balta-Calleja, F.J. (1988) Microstructural Changes in Polyethylene-Polypropylene Blends as Revealed by Microhardness. Journal of Materials Science, 23, 862-866. https://doi.org/10.1007/BF01153980
- Fischer E.W. and Fakirov, S. (1976) Structure and Properties of Polyethyleneterephthalate Crystallized by Annealing in the Highly Oriented State. Part 1 Morphological Structure as Revealed by Small-Angle X-Ray Scattering. Journal of Materials Science, 11, 1041-1065. https://doi.org/10.1007/BF02396639
- Weon, J. (2009) Effects of Thermal Ageing on Mechanical and Thermal Behaviors of Linear Low Density Polyethylene Pipe. Polymer Degradation and Stability, 95, 14-20. https://doi.org/10.1016/j.polymdegradstab.2009.10.016